We have advanced equipment. Our products are exported to the USA, the UK and so on, enjoying a good reputation among customers for False Ceiling T Bar , Rock Wool Blanket 70kg M3 , Anodized Aluminum Profiles , Many years of work experience, we have realized the importance of providing good quality products and the best before-sales and after-sales services.
Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua Detail:

In building materials, it is used as a water-retaining agent and retarder for cement sludge with pumpability. It can be used as a binder in plaster, gypsum, inverted powder or other building materials to improve spreadability and prolong operation time. It can be used as an agent for sticking bricks, tiles, marbles, plastic decorations, and bonding intensifiers. It can also reduce the amount of cement. The water retention of HPMC prevents the slurry from cracking due to drying too fast after coating, and enhances the strength after hardening.

In addition, it is used as thickener, stability, emulsifier, excipient, water retention in the production of other petrochemicals, coatings, building materials, paint removers, agricultural chemicals, inks, textile printing and dyeing, ceramics, papermaking, and cosmetic brands. Agent, film-forming agent, etc.

1. Appearance: white or almost white powder, odorless and tasteless.

2. Granularity: 10 mesh pass rate is greater than 98.5%; 80 mesh pass rate is greater than 100%.

3. Carbonization temperature: 280-300℃.

4. Room density: 0.25-0.7G/CM3 (usually about 0.5G/CM3), the specific gravity is 1.26-1.31.

5. Discoloration temperature: 190-200℃.

6. Natural temperature: about 360℃.

 

Production Method

The refined cotton cellulose is treated with lye at 35-40°C for half an hour, squeezed, the cellulose is crushed, and properly aged at 35°C, so that the obtained alkali fiber average degree of polymerization is within the required range. Put the alkali fiber into the etherification kettle, add propylene oxide and methyl chloride successively, and etherify at 50-80℃ for 5h, the maximum pressure is about 1.8MPa. Then add proper amount of hydrochloric acid and oxalic acid to wash materials in hot water at 90°C to increase the volume. Dehydrate with a centrifuge. Wash to neutral. When the water content in the material is less than 60%, dry it with a stream of hot air at 130℃ to less than 5%. Finally, it is crushed through a 20-mesh sieve to obtain the finished product.

 


Product detail pictures:

Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose  HPMC – Beihua detail pictures


Related Product Guide:

We pursue the management tenet of "Quality is superior, Service is supreme, Reputation is first", and will sincerely create and share success with all clients for Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua , The product will supply to all over the world, such as: New York, Singapore, Anguilla, We have a good reputation for stable quality products, well received by customers at home and abroad. Our company would be guided by the idea of "Standing in Domestic Markets, Walking into International Markets". We sincerely hope that we could do business with customers both at home and abroad. We expect sincere cooperation and common development!
  • It is a very good, very rare business partners, looking forward to the next more perfect cooperation!
    5 Stars By Laura from Munich - 2018.06.18 19:26
    This enterprise in the industry is strong and competitive, advancing with the times and develop sustainable, we are very pleased to have a opportunity to cooperate!
    5 Stars By Philipppa from Italy - 2018.02.12 14:52
    Write your message here and send it to us