We have now a hugely efficient team to deal with inquiries from buyers. Our goal is "100% client gratification by our solution high-quality, rate & our team service" and take pleasure in a great popularity among clients. With several factories, we will provide a wide assortment of Building Materials , Rock Wool Piping , Roll Blanket , Together with the everlasting target of "continuous top quality improvement, customer satisfaction", we have been sure that our products high quality is stable and trustworthy and our solutions are best-selling at your home and overseas.
Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua Detail:

In building materials, it is used as a water-retaining agent and retarder for cement sludge with pumpability. It can be used as a binder in plaster, gypsum, inverted powder or other building materials to improve spreadability and prolong operation time. It can be used as an agent for sticking bricks, tiles, marbles, plastic decorations, and bonding intensifiers. It can also reduce the amount of cement. The water retention of HPMC prevents the slurry from cracking due to drying too fast after coating, and enhances the strength after hardening.

In addition, it is used as thickener, stability, emulsifier, excipient, water retention in the production of other petrochemicals, coatings, building materials, paint removers, agricultural chemicals, inks, textile printing and dyeing, ceramics, papermaking, and cosmetic brands. Agent, film-forming agent, etc.

1. Appearance: white or almost white powder, odorless and tasteless.

2. Granularity: 10 mesh pass rate is greater than 98.5%; 80 mesh pass rate is greater than 100%.

3. Carbonization temperature: 280-300℃.

4. Room density: 0.25-0.7G/CM3 (usually about 0.5G/CM3), the specific gravity is 1.26-1.31.

5. Discoloration temperature: 190-200℃.

6. Natural temperature: about 360℃.

 

Production Method

The refined cotton cellulose is treated with lye at 35-40°C for half an hour, squeezed, the cellulose is crushed, and properly aged at 35°C, so that the obtained alkali fiber average degree of polymerization is within the required range. Put the alkali fiber into the etherification kettle, add propylene oxide and methyl chloride successively, and etherify at 50-80℃ for 5h, the maximum pressure is about 1.8MPa. Then add proper amount of hydrochloric acid and oxalic acid to wash materials in hot water at 90°C to increase the volume. Dehydrate with a centrifuge. Wash to neutral. When the water content in the material is less than 60%, dry it with a stream of hot air at 130℃ to less than 5%. Finally, it is crushed through a 20-mesh sieve to obtain the finished product.

 


Product detail pictures:

Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose  HPMC – Beihua detail pictures


Related Product Guide:

We've been committed to offering easy,time-saving and money-saving one-stop purchasing support of consumer for Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua , The product will supply to all over the world, such as: Serbia, Belize, Guyana, Now, we professionally supplies customers with our main merchandise And our business is not only the "buy" and "sell", but also focus on more. We target to be your loyal supplier and long-term cooperator in China. Now, We hope to be the friends with you.
  • Staff is skilled, well-equipped, process is specification, products meet the requirements and delivery is guaranteed, a best partner!
    5 Stars By Dora from Haiti - 2017.09.30 16:36
    The customer service staff's answer is very meticulous, the most important is that the product quality is very good, and packaged carefully, shipped quickly!
    5 Stars By Nicci Hackner from Plymouth - 2018.06.18 19:26
    Write your message here and send it to us