Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua

short description:


Product Detail

Product Tags

Related Video

Feedback (2)

No matter new customer or previous client, We believe in prolonged time period and trustworthy relationship for Stainless Steel V-Shape Angle , Tee Grids , L Type Wall Angle , We, with open arms, invite all interested buyers to visit our website or contact us directly for further information.
Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua Detail:

In building materials, it is used as a water-retaining agent and retarder for cement sludge with pumpability. It can be used as a binder in plaster, gypsum, inverted powder or other building materials to improve spreadability and prolong operation time. It can be used as an agent for sticking bricks, tiles, marbles, plastic decorations, and bonding intensifiers. It can also reduce the amount of cement. The water retention of HPMC prevents the slurry from cracking due to drying too fast after coating, and enhances the strength after hardening.

In addition, it is used as thickener, stability, emulsifier, excipient, water retention in the production of other petrochemicals, coatings, building materials, paint removers, agricultural chemicals, inks, textile printing and dyeing, ceramics, papermaking, and cosmetic brands. Agent, film-forming agent, etc.

1. Appearance: white or almost white powder, odorless and tasteless.

2. Granularity: 10 mesh pass rate is greater than 98.5%; 80 mesh pass rate is greater than 100%.

3. Carbonization temperature: 280-300℃.

4. Room density: 0.25-0.7G/CM3 (usually about 0.5G/CM3), the specific gravity is 1.26-1.31.

5. Discoloration temperature: 190-200℃.

6. Natural temperature: about 360℃.

 

Production Method

The refined cotton cellulose is treated with lye at 35-40°C for half an hour, squeezed, the cellulose is crushed, and properly aged at 35°C, so that the obtained alkali fiber average degree of polymerization is within the required range. Put the alkali fiber into the etherification kettle, add propylene oxide and methyl chloride successively, and etherify at 50-80℃ for 5h, the maximum pressure is about 1.8MPa. Then add proper amount of hydrochloric acid and oxalic acid to wash materials in hot water at 90°C to increase the volume. Dehydrate with a centrifuge. Wash to neutral. When the water content in the material is less than 60%, dry it with a stream of hot air at 130℃ to less than 5%. Finally, it is crushed through a 20-mesh sieve to obtain the finished product.

 


Product detail pictures:

Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose  HPMC – Beihua detail pictures


Related Product Guide:

In order to best meet client's needs, all of our operations are strictly performed in line with our motto "High Quality, Competitive Price, Fast Service" for Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua , The product will supply to all over the world, such as: Luxemburg, Saudi Arabia, Berlin, We provide good quality but unbeatable low price and the best service. Welcome to post your samples and color ring to us .We will produce the goods according to your request. If you are interested in any products we offer, please feel free to contact us directly by mail, fax, telephone or internet. We are here to answer your questions from Monday to Saturday and looking forward to cooperating with you.
  • This manufacturers not only respected our choice and requirements, but also gave us a lot of good suggestions, ultimately, we successfully completed the procurement tasks.
    5 Stars By Daisy from Bhutan - 2017.09.26 12:12
    This is a reputable company, they have a high level of business management, good quality product and service, every cooperation is assured and delighted!
    5 Stars By Elma from Liberia - 2017.12.31 14:53
    Write your message here and send it to us