head_bg

products

Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua

short description:


Product Detail

Product Tags

Related Video

Feedback (2)

The business keeps to the operation concept "scientific management, premium quality and efficiency primacy, customer supreme for Pvc Panel , Drywall Perforated Angle , Handmade Cleanroom Panel , We always provide best quality products and excellent service for the majority of business users and traders . Warmly welcome to join us, let's innovate together, and fly dreams.
Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua Detail:

In building materials, it is used as a water-retaining agent and retarder for cement sludge with pumpability. It can be used as a binder in plaster, gypsum, inverted powder or other building materials to improve spreadability and prolong operation time. It can be used as an agent for sticking bricks, tiles, marbles, plastic decorations, and bonding intensifiers. It can also reduce the amount of cement. The water retention of HPMC prevents the slurry from cracking due to drying too fast after coating, and enhances the strength after hardening.

In addition, it is used as thickener, stability, emulsifier, excipient, water retention in the production of other petrochemicals, coatings, building materials, paint removers, agricultural chemicals, inks, textile printing and dyeing, ceramics, papermaking, and cosmetic brands. Agent, film-forming agent, etc.

1. Appearance: white or almost white powder, odorless and tasteless.

2. Granularity: 10 mesh pass rate is greater than 98.5%; 80 mesh pass rate is greater than 100%.

3. Carbonization temperature: 280-300℃.

4. Room density: 0.25-0.7G/CM3 (usually about 0.5G/CM3), the specific gravity is 1.26-1.31.

5. Discoloration temperature: 190-200℃.

6. Natural temperature: about 360℃.

 

Production Method

The refined cotton cellulose is treated with lye at 35-40°C for half an hour, squeezed, the cellulose is crushed, and properly aged at 35°C, so that the obtained alkali fiber average degree of polymerization is within the required range. Put the alkali fiber into the etherification kettle, add propylene oxide and methyl chloride successively, and etherify at 50-80℃ for 5h, the maximum pressure is about 1.8MPa. Then add proper amount of hydrochloric acid and oxalic acid to wash materials in hot water at 90°C to increase the volume. Dehydrate with a centrifuge. Wash to neutral. When the water content in the material is less than 60%, dry it with a stream of hot air at 130℃ to less than 5%. Finally, it is crushed through a 20-mesh sieve to obtain the finished product.

 


Product detail pictures:

Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose  HPMC – Beihua detail pictures


Related Product Guide:

To create more benefit for buyers is our business philosophy; shopper growing is our working chase for Short Lead Time for Mineral Wool Board - Hydroxypropyl Methylcellulose HPMC – Beihua , The product will supply to all over the world, such as: Malta, Eindhoven, Ukraine, We've been adhering to the philosophy of "attracting customers with the best items and excellent service". We welcome customers, business associations and friends from all parts of the world to contact us and seek cooperation for mutual benefits.
  • The factory technical staff not only have high level of technology, their English level is also very good, this is a great help to technology communication.
    5 Stars By Yannick Vergoz from Sydney - 2018.06.05 13:10
    Production management mechanism is completed, quality is guaranteed, high credibility and service let the cooperation is easy, perfect!
    5 Stars By Annabelle from America - 2017.11.20 15:58
    Write your message here and send it to us